Improvement of tensile shear strength and wood failure percentage of 1C PUR bonded wooden joints at wet stage by means of DMF priming
Kläusler, Oliver, Hass, Philipp, Amen, Carlos, Schlegel, Sven, Niemz, PeterТом: